Default 5.3 header tank galvanising

Has anyone had or tried having their header tank galvanised? Think it would be ok regarding temperatures and the sensor hole would use as a vent/drain hole for the galvanisers. Just a thought to try to slow the rusting process. Any ideas welcome thanks.
 
  #2  
Old 12-02-2017, 11:34 AM
Daim's Avatar
Veteran Member
Join Date: May 2014
Location: Bremen, Germany
Posts: 5,906
Received 2,181 Likes on 1,584 Posts
Default

A proper galvanizer won't do it.

1st: because they use multiple fluids/acids which need to be drained quickly or will destroy the material
2nd: it is brazed in certain areas.

If you use the proper antifreeze, it won't rust. That also means to regularly replace/change the fluid/coolant.
 
  #3  
Old 12-02-2017, 11:51 AM
brinny's Avatar
Veteran Member
Thread Starter
Join Date: Sep 2015
Location: Yorkshire U.K.
Posts: 1,303
Received 426 Likes on 252 Posts
Default

Last time I went to the galvanisers with some products he told me they pickled things for 24 hours before galvanising so no rush there. Brazing is done at a much higher temperature than zinc melts at so I didn't think that would be a problem either. The big hole in my inner wing leads me to believe anti freeze is not sufficient which is why I wanted to try other ideas.?
 
  #4  
Old 12-02-2017, 12:31 PM
Doug's Avatar
Veteran Member
Join Date: Mar 2008
Location: Pacific Northwest USA
Posts: 24,927
Received 10,988 Likes on 7,215 Posts
Default

No advice or comment on galvanizing. I'm not well enough informed. But that never stops me from rambling a bit

My guess is that, often as not, the header tanks are neglected. They don't get a good cleaning from time-to-time as (hopefully) the rest of the cooling system does. Gloppy stuff accumulates and promotes rot. Personally I take mine to the local radiator shop for a boil-out. After that, DIY cleaning every 2-3 years keeps 'em clean.

I've also seen a couple cars where the tank (and inner fender) have rotted due to a water-trapping build-up of debris between the tank and the inner fender.

Cheers
DD
 
  #5  
Old 12-02-2017, 03:24 PM
warrjon's Avatar
Veteran Member
Join Date: May 2010
Location: Vic Australia
Posts: 4,638
Received 2,576 Likes on 1,712 Posts
Default

I bought a stainless steel one and X over pipe. I have seen them on eBay. Or you could have a radiator shop make on from aluminium.
 
The following users liked this post:
Greg in France (12-03-2017)
  #6  
Old 12-03-2017, 02:23 AM
Greg in France's Avatar
Veteran Member
Join Date: Jan 2012
Location: France
Posts: 13,612
Received 9,440 Likes on 5,525 Posts
Default

Brinny
There are loads of one-man stainless fabricators in England, ditto ally. If you look one up and give them a sample, I am sure you will get one pretty reasonably priced. You can buy radiator cap necks no bother, which is the only specialised part, so that can be supplied to the fabricator. I used this firm, who were really good, but I am sure you can find someone locally.

Unit 7 Creations Ltd.
Unit 6, 57 Thorby Avenue,
March Trading Park,
March, Cambridgeshire,
PE15 0AR
Tel Office: (+44) 01354-655-886
Mobile: (+44) 0788-665-7762



Greg
 
  #7  
Old 12-03-2017, 02:57 AM
Daim's Avatar
Veteran Member
Join Date: May 2014
Location: Bremen, Germany
Posts: 5,906
Received 2,181 Likes on 1,584 Posts
Default

Originally Posted by brinny
Last time I went to the galvanisers with some products he told me they pickled things for 24 hours before galvanising so no rush there. Brazing is done at a much higher temperature than zinc melts at so I didn't think that would be a problem either. The big hole in my inner wing leads me to believe anti freeze is not sufficient which is why I wanted to try other ideas.?
It's not the time IN the bath but the time BETWEEN the baths. As it will go through several baths, and galvanizers don't have hours to wait for something to drain, it has to go quickly. I had 2 transmission pipes ans the fuel rail zinc plated. Both were only just possible, as the fluid would drain well.

At least here, where they use more 'ecological' fluids, the fluids can react quite nastily of not drained sufficiently. As a comparission: I have an old header tank here. I removed it in spring 2016. It still has fluid in it. I don't know why, maybe too much sludge, but it might have a baffle or so inside.

I simply bought a new one for like £70 if at all...
 
  #8  
Old 12-03-2017, 06:36 AM
Join Date: Feb 2010
Location: Adelaide Stralia
Posts: 27,776
Received 10,589 Likes on 6,994 Posts
Default

Get a stainless header tank.

Thats all we get down here as Jag replacements, and mine has been there since 1994.

Like Warren, and NO issues at all.
 
  #9  
Old 12-03-2017, 11:36 AM
orangeblossom's Avatar
Veteran Member
Join Date: Feb 2013
Posts: 17,711
Received 3,858 Likes on 2,669 Posts
Default

Hi Brinny

While I'm a Big Fan of Galvanizing and have had the Chassis on my Land Rover done and also the Front Beam of my MGB.

Galvanizing the Header Tank, would be something that I would not risk in case any Zinc deposits blocked the Waterways in the Engine.

Or set up some sort of adverse Chemical Reaction.

So I agree with the others who've said, go for Stainless Steel or Aluminum, which is what I am going to do if/when my Header starts leaking.

Which should also be much cheaper than buying OEM there are loads of these Tanks on ebay and one of them could make a better replacement.


Galvanized Front Beam for my MGB
 
  #10  
Old 12-03-2017, 12:19 PM
brinny's Avatar
Veteran Member
Thread Starter
Join Date: Sep 2015
Location: Yorkshire U.K.
Posts: 1,303
Received 426 Likes on 252 Posts
Default

Thanks for the input lads
 

Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 



All times are GMT -5. The time now is 09:25 PM.